Daniel WereeHave been business relationship for 3 years, great partner for Nickel Cobalt Alloy!
-
Carolina FasioOn-time delivery. And support is good and fast.
Inconel X-750 Nickel Alloy Precipitation-hardened Superalloy up to 800°C Application

Contact me for free samples and coupons.
WhatsApp:0086 18588475571
Wechat: 0086 18588475571
Skype: sales10@aixton.com
If you have any concern, we provide 24-hour online help.
xEqual Grades | Inconel X-750, NiCr15Fe7TiAl, 2.4669,UNS N07750 | Melting Range | 1395°C~1425°C |
---|---|---|---|
Density | 8.25g/cm3 | Forms Of Supply | Plate, Strip, Bar, Forging, Ring, Wire, Tube |
Spec | GB/T 14992 | Product Name | Nickel Cobalt Alloy |
Highlight | nickel based alloys,high temperature nickel alloys |
Inconel X-750 Nickel Alloy Precipitation-hardened Superalloy up to 800°C Application
Inconel X-750 is a precipitation-hardenable nickel-chromium alloy used for its corrosion and oxidation resistance and high strength at temperatures up to 1300°F. Although much of the effect of precipitation hardening is lost with increasing temperature over 1300°F, heat-treated material has useful strength up to 1800°F. GH4145 also has excellent properties down to cryogenic termperatures.
Depending on the application and the properties desired, various heat treatments are employed. For service above 1100°F, particularly where loads are to be sustained for long times, optimum properties are achieved by solution treating (2100°F) plus stabilization treating (1550°F) plus precipitation treating (1300°F). For service below 1100°F, the alloy may be strengthened by precipitation treating after hot or cold working or by precipitation treating after equalizing or solution treating. A furnace-cooling treatment is also used to develop optimum properties for some applications.
Chemical compositin
Element | C | Cr | Ni | Co | Al | Ti | Fe | Nb | Mn | Si | S | P | Cu |
Weight(%) | 0.08 max | 14.00~17.00 | 70.00 min | 1.00 max | 0.40~1.00 | 2.25~2.75 | 5.00~9.00 | 0.70~1.20 | 1.00 max | 0.50 max | 0.010 max | 0.015 max | 0.50 max |
Features
- Good creep rupture strength at high temperatures
- Not as strong as Nimonic 90
- Very good at cryogenic temperatures
- Age hardenable
- High temperature dynamic applications
Applications
- Nuclear reactors
- Gas turbines
- Rocket engines
- Pressure vessels
- Aircraft structures
Available Product Forms
Sheet, strip, plate, round bar, flat bar, forging stock, hexagon, wire, tube and extruded
About XUNSHI
Suzhou Xunshi New Material Co. Ltd- referred as XUNSHI hereafter, is a professional manufacturer of high-performance alloy products. XUNSHI is engaged in supplying high quality and cost-effective Superalloy, Anti-Corrosion Alloy, Precision Alloy, Special Stainless Steel and Magnetostrictive Material to customers worldwide.
Why XUNSHI
· Highly experienced in alloy industry
· Top experts of industry in China
· Advanced technology and process from top famous institutes in China
· Advanced devices through whole production and inspection process
· Strict quality control system
· Company motto: best service, most value
· Smart sales policy
Service Items of XUNSHI
· Non-standard product research and pre-production
· Fabrication of products
· Cutting, splitting for sheets and plates in stock
· Heat treatment (Solution treatment, aging harden treatment, anneal, spring temper, quench etc.)
· Surface finish (peeling, gridding, polishing)
· Logistics service
· Customized packing service (also for exporting)
· Import and export (XUNSHI is certificated)
· Document translation
· Hard-to-find material sourcing
Customers of XUNSHI
Customers of XUNSHI are all over China (Taiwan and Hong Kong included). And we are exporting to USA, Canada, Italy, UK, Poland, Greece, Russia, Turkey, Iran, Israel, South Africa, South Korea, North Korea, India, Argentina, and Brazil and so on. Customers from 30+ countries trust us.
Where is XUNSHI
A- XUNSHI is in Huaqiao, Kunshan, 215332 China, which is very closed to Shanghai.
B- Xunshi is around 80KM from Shanghai Pudong International Airport (PVG).
C- 20KM from Shanghai Hongqiao Airport
D- 20KM from Shanghai Hongqiao Railway Station
E- You can contact XUNSHI sales for a pickup service.